The Longer LK5 Pro is an FDM 3D printer from Longer with a 300 x 300 x 400 mm build volume.
The Longer LK5 Pro is an FDM 3D printer from Longer with a 300 x 300 x 400 mm build volume.
Calibrating the Longer LK5 Pro is essential for achieving optimal print quality and reliability. Below is a step-by-step guide to calibrate the printer, including detailed explanations of each step and engineering insights.
Process: Begin by ensuring the printer is on a flat, stable surface. Use the BLTouch auto-leveling sensor to measure the bed’s flatness. Access the printer’s menu and navigate to the "Leveling" section.
Symptom: Users have reported inconsistent extrusion and layer shifting during high-speed prints.
Cause: The dual-gear extruder system can slip under high-torque conditions, especially with flexible filaments. Additionally, the delta-style kinematics may experience misalignment if the diagonal rods are not perfectly tensioned.
Solution: Replace the extruder gears with hardened steel versions for better grip.
The Longer LK5 Pro excels in scenarios requiring large build volumes and moderate print speeds. It is ideal for prototyping, educational institutions, and hobbyists who need a reliable printer for everyday use. The printer’s delta kinematics make it suitable for applications like:.
| Manufacturer | Longer |
|---|---|
| Technology | FDM |
| Class | hobby |
| Build volume | 300 x 300 x 400 mm |
| Auto levelling | no |
| Compatible materials | pla, petg, tpu, matte-pla, silk-pla, glow-pla, pva, wood |
| Manufacturer | Longer |
|---|---|
| Technology | FDM |
| Class | hobby |
| Build volume | 300 x 300 x 400 mm |
| Auto levelling | no |
same class and kinematics, close in price within 30 percent
| Model | Class | Build volume |
|---|---|---|
| Longer LK5 Pro (this) | hobby | 300 x 300 x 400 mm |
| Alfawise U20 | hobby | 300 x 300 x 400 mm |
| Anet E10 | hobby | 300 x 300 x 400 mm |
| Anet E12 | hobby | 300 x 300 x 400 mm |
| Material | Nozzle temperature | Bed temperature |
|---|---|---|
| PLA | 210-230 °C | 55-65 °C |
| PETG | 230-265 °C | 70-85 °C |
| TPU | 220-240 °C | 35-55 °C |
| PVA | 220-240 °C | 45-65 °C |