up to 250°C HDT. engineering prototypes under heat. requires heat post-cure.
When you need detail of resin + heat resistance. Injection mold inserts (low-volume), engine bay prototypes, heated assembly fixtures.
| Formula | modified methacrylate |
|---|---|
| Density | 1.18 g/cm³ |
| Tg (glass transition) | 200°C |
| Nozzle temp | 0–0°C |
| Bed temp | 0–0°C |
| Enclosure | wash + cure station |
| Difficulty | ★★★★: advanced |
Engineer, author of The Big Book of 3D Printing and additive manufacturing expert
| Formula | modified methacrylate |
|---|---|
| Density (g/cm³) | 1.18 |
| Tg (°C) | 200 |
| Print ease (0-10) | 4 |
| Tensile (0-10) | 7 |
| Flexibility (0-10) | 2 |
| Impact resistance (0-10) | 4 |
| Heat resistance (0-10) | 9 |
| UV resistance (0-10) | 3 |
| Chemical resistance (0-10) | 6 |
| Cost (0-10) | 2 |
| Safety (0-10) | 4 |
| Finishing (0-10) | 9 |
| Bed adhesion (0-10) | 8 |
| Accuracy (0-10) | 9 |
| Property | High-Temp Resin | Castable Resin | Dental Resin | Flexible Resin |
|---|---|---|---|---|
| Print ease | 4 | 4 | 5 | 4 |
| Tensile | 7 | 3 | 6 | 4 |
| Flexibility | 2 | 2 | 3 | 9 |
| Impact resistance | 4 | 2 | 5 | 8 |
| Heat resistance | 9 | 1 | 6 | 3 |
| UV resistance | 3 | 2 | 5 | 2 |
| Chemical resistance | 6 | 3 | 7 | 4 |
| Cost | 2 | 3 | 1 | 5 |
| Safety | 4 | 4 | 10 | 4 |
| Finishing | 9 | 10 | 10 | 8 |
| Bed adhesion | 8 | 7 | 8 | 7 |
| Accuracy | 9 | 10 | 10 | 7 |
Compatible printers: 90