In 2025–2026, low-energy sintering for Metal Binder Jetting reduces the most energy-intensive step in BJ workflow. Standard sintering at 1200–1400°C for 4–12 hours is being optimized.
Standard Sintering Parameters
| Parameter | 316L Steel | Ti-6Al-4V |
|---|---|---|
| Temperature | 1360–1380°C | 1250–1350°C |
| Duration | 6–12 hours | 4–8 hours |
| Shrinkage | 17–20% | 15–18% |
Interactive Filament Selector
Answer 3 quick questions and find the optimal material for your project.
1. What are the mechanical requirements for the part?
2. What temperature will the part operate at?
3. Are there any specific environmental requirements?
Our recommendation:
PLA filament
Ideal for easy printing, model visualization and decorative parts.
Low-Energy Strategies
- Microwave-Assisted (30–50% faster). 2. Spark Plasma Sintering (minutes vs hours). 3. Two-Step Sintering. 4. Optimized Binder Chemistry.
FAQ
Interactive Analyzer for Low-Energy Sintering Strategies For Metal Binder Jetting
Select a profile to view detailed analysis.
The full picture
This article is one page from The Big Book of 3D Printing: 704 illustrated pages covering every technology, material and fix in one reference.
Read it on Kindle →Engineer, author of The Big Book of 3D Printing and additive manufacturing expert