Nylon (polyamide) is the engineering filament that makes the difference between ‘3D printed prototype’ and ‘functional production part’. It’s tough, flexible, wear-resistant, and works well under mechanical load. Nylon is the choice for gears, bearing housings, hook-and-loop fasteners, drone arms, and anything that will move and grind. But nylon comes with problems: it absorbs moisture more aggressively than any other common FDM plastic, requires high print temperature (250-280°C), and doesn’t tolerate damp environments without an enclosure. In this guide we’ll show how to print nylon reliably, from PA6 to carbon-fiber-filled PA-CF.
Types of nylon, PA6, PA12, PA-CF
PA12 (polyamide 12): most used nylon for FDM. Melting around 175°C (prints at 240-260°C), tensile strength 50 MPa, absorbs moisture less than PA6. Suitable for most engineering applications.
PA6 (polyamide 6): tougher and more wear-resistant than PA12. Tensile strength 70-80 MPa. Prints at 270-290°C. Absorbs moisture extremely quickly, without active drying not recommended.
PA-CF (carbon-fiber-filled nylon): nylon with 15-30% carbon fiber. Exceptionally tough and rigid, less warping than pure nylon, excellent for drones and engineering parts under mechanical load. Prints at 280-300°C, abrades brass nozzles quickly: needs hardened steel nozzle. €60-€90/kg.
PA-GF (glass-fiber-filled): alternative to PA-CF, cheaper (€40-€50/kg), similar stiffness, but more brittle on impact.
For most users: PA12 is the starting choice. PA-CF comes when you have experience and need extreme stiffness.
Recommended FDM printers
Bambu Lab X1-Carbon (€1449): enclosed chamber and hardened nozzle come standard. Recommended for most nylon work.
Prusa MK4 with Prusa Enclosure (€999 + €330): open-source, excellent build quality. With hardened nozzle upgrade (€30): ready for PA-CF.
Qidi Plus 4 (€650): heated chamber to 65°C, hardened hotend. Recommended for production nylon work.
Markforged Mark Two/X7: professional choice for continuous-fiber-reinforced nylon. Prices €15,000+. Recommended for industrial clients.
Avoid: open-frame printers like stock Ender 3, nylon WILL warp in open chamber. Bambu A1 is also open frame; for nylon, X1-Carbon is necessary.
Recommended nylon brands
Polymaker PolyMide PA612: balanced nylon. €45-€55/kg. Recommended to start.
Taulman 645 Bridge: pioneer nylon for FDM. Global reputation for quality. €50-€60/kg.
Fiberlogy Nylon PA12: Polish brand, good quality, €35-€45/kg. Recommended for budget-conscious buyers.
Bambu Lab PAHT-CF: high-temperature carbon-fiber nylon, optimized for X1-Carbon. €70/kg.
Nanovia PA-CF: premium carbon-fiber nylon, €80-€100/kg. Recommended for drone and automotive parts.
Markforged Onyx (PA-CF): only for Markforged printers. Industrial gold standard.
Avoid: unbranded nylon. Differences in moisture absorption between batches make consistent print impossible.
Optimal settings for PA12
Nozzle temperature: 250-270°C. PA-CF: 270-290°C. Start in the middle and adjust ±5°C.
Bed temperature: 70-90°C. Garolite (special bed material) or PEI with slurry give best adhesion for nylon.
Chamber temperature: 40-50°C minimum. Without heated chamber: printing not recommended.
Speed: 30-60 mm/s. Under-extrusion is common at high speeds with nylon (high viscosity).
Cooling: 0-30%. Nylon loves slow cooling for good layer adhesion. First 10 layers: no cooling.
Layer height: 0.20-0.25 mm.
Retraction: 1-2 mm Direct Drive, 4-6 mm Bowden. Speed 30 mm/s.
Drying: CRITICAL for nylon. Dry filament 6-12 hours at 70-80°C before print. Wet nylon makes white bubbles in print and brittle layers. Inline filament dryer (PrintDry, SUNLU FilaDryer) is a recommended investment.
Common mistakes
Bubbles in print, brittle layers: wet filament. Dry 8 hours at 70°C. Place spool directly in filament dryer for print, not outside.
Warping: chamber too cool. Close bay door, add insulating panels, or move printer to a warmer room. 10mm brim mandatory.
Layer separation: nozzle temperature too low, or cooling too high. PA12 often wants 260-270°C, not the stock 240°C.
Delamination between infill and perimeters: nozzle temperature for PA-CF should be +10°C above pure PA12. Carbon fiber wicks heat: the material cools too fast.
Nozzle wear (on brass nozzles with PA-CF): switch brass to hardened steel nozzle (Bambu hardened, E3D Nozzle X). Brass wears out in 5-10 PA-CF print sessions.
Frequently Asked Questions (FAQ)
Interactive Analyzer for Fdm With Nylon (Pa), The Engineering Standard
Select a profile to view detailed analysis.
The full picture
This article is one page from The Big Book of 3D Printing: 704 illustrated pages covering every technology, material and fix in one reference.
Read it on Kindle →Engineer, author of The Big Book of 3D Printing and additive manufacturing expert