IT▾
EduFacturing · Stampa 3D

Impostazioni Slicer per 16 Materiali FDM (2026)

Temperature consigliate per ugello, piatto e camera, velocità ventola e requisito di chiusura: un consenso pratico tra PrusaSlicer, Bambu Studio e Cura.

MaterialeUgello °CPiatto °CCamera °CVentolaChiusura richiesta
PLA195–21550–60–100%no
PLA Pro / PLA+210–23055–65–80%no
PLA Silk205–22550–60–100%no
PETG230–25070–85–50%no
PETG-CF (Carbon)240–26075–9040–50°C50%sì
ABS240–26095–11040–55°C0%sì
ASA240–26095–11040–55°C0%sì
TPU 95A220–24040–60–50%no
TPU 85A (super soft)225–24530–50–30%no
Nylon PA12 / PA6240–27070–9040–60°C30%sì
PA-CF (Carbon Nylon)260–29080–10050–70°C30%sì
PA-GF (Glass-fiber Nylon)255–28580–10050–70°C30%sì
PC (Polycarbonate)270–310110–13060–80°C0%sì
PET-CF (Carbon PET)270–30080–10050–70°C30%sì
PEEK380–430120–16080–130°C0%sì
PEI / Ultem 9085370–410140–180120–180°C0%sì

Licenza: CC BY 4.0 · Dataset citabile: DOI 10.5281/zenodo.20551933

Domande frequenti

Qual è la temperatura ugello per PLA?
PLA stampa a 195–215 °C all'ugello e 50–60 °C al piatto, con ventola al 100 % e senza camera chiusa.
Ho bisogno di una camera chiusa per ABS o ASA?
Sì. ABS e ASA tendono a deformarsi; una camera chiusa a 40–55 °C mantiene la temperatura stabile, e la ventola rimane allo 0 %.
Quali impostazioni per PETG?
PETG: ugello 230–250 °C, piatto 70–85 °C, ventola circa 50 %. Chiusura non necessaria.
Quali materiali richiedono le temperature più elevate?
PEEK (ugello 380–430 °C, camera 80–130 °C) e PEI/Ultem 9085 (370–410 °C, camera 120–180 °C) richiedono stampanti ad alta temperatura con camera riscaldata.