Спецификации
- Производител: Sovol 3D
- Технология: FDM
- Клас: experimenter
Чести проблеми и решения
Stringing
Thin, web-like plastic threads appearing between separate parts of the printed model. Решение: Dry the filament for 4-6 hours at 50°C, increase retraction distance by 1-2 mm, reduce nozzle temperature by 5°C, and increase travel speed to 200 mm/s.
Warping
The corners or edges of the print detach from the build plate and curl upwards due to rapid, uneven cooling and thermal stress. Решение: Increase bed temperature by 5°C, add a 5-10 mm brim, apply an adhesive like a glue stick, and reduce part cooling to 30% for the first 5 layers.
Elephant’s Foot
The bottom layer of the print is excessively squished and expands outward beyond the designated CAD dimensions. Решение: Raise the Z-offset by +0.05 mm, decrease the bed temperature by 5°C specifically for the first layer, and enable software compensation of 0.1-0.2 mm.
Layer Shift
The upper layers of the print are suddenly shifted horizontally relative to the lower layers. Решение: Hardware-tighten the X and Y axis belts, check the grub screws on the stepper motor pulleys, and reduce print speed by 20%.
Инженер, автор на „Голямата книга на 3D принтирането“ и експерт по адитивни технологии
Обновено на 21 септември 2026
Този текст е написан с помощта на AI; фактите са сверени с източниците на 21 септември 2026.