PA12 (SLS) Slicer Settings
SLS · Common
Last updated: 2026
For PA12 (SLS) (SLS): chamber temperature 165–175°C, layer height 0.1–0.15 mm. SLS needs no supports: the powder holds the part.
Recommended settings
| Chamber temperature | 165–175 °C |
| Layer height | 0.1–0.15 mm |
| Supports | not needed (powder holds the part) |
| Popular brands | EOS PA2200, HP 3D HR PA12, Sinterit |
No supports → full geometric freedom. Powder refresh ratio 30–50% fresh/recycled.
Frequently asked questions
What chamber temperature for PA12 (SLS)?
Chamber 165–175°C, layer height 0.1–0.15 mm.
Do I need supports for PA12 (SLS)?
No. In SLS the unsintered powder supports the part, so no supports are needed: complex geometries are possible.
See 3D printing costs →