Dental / Bio Resin Slicer Settings

SLA · Specialty

Last updated: 2026

For Dental / Bio Resin (SLA/LCD): exposure 30s (first layer) / 2.8s (normal), layer height 0.025–0.05 mm, IPA wash 10 min, UV cure 30 min at 80°C, shrinkage ~0.5%.

Recommended settings

Layer height0.025–0.05 mm
Exposure (first layer)30 s
Exposure (normal layer)2.8 s
IPA wash10 min
UV cure30 min at 80°C
Shrinkage after cure~0.5%
Common defectsBiocompatibility requires STRICT post-cure; under-cure = leaching of unreacted monomers
Popular brandsFormlabs Dental, NextDent, Asiga
ISO 10993 biocompatible. Vertical orientation matters for dental models. Validated workflow only.

Frequently asked questions

What exposure for Dental / Bio Resin?

First layer 30s, normal layer 2.8s, layer height 0.025–0.05 mm.

How much UV cure for Dental / Bio Resin?

30 minutes at 80°C after 10 min IPA wash.

See 3D printing costs →