FDM · Engineering
Last updated: 2026
| Nozzle temperature | 240–260 °C |
| Bed temperature | 95–110 °C |
| Chamber temperature | 40–55 °C |
| Layer height | 0.16–0.24 mm |
| Retraction | 2 mm at 40 mm/s |
| Cooling fan | 0% |
| Infill | 30% |
| Bed adhesion | brim |
| Enclosure | yes |
| Hardened nozzle | no |
| All-metal hotend | no |
| Popular brands | Polymaker, Prusament, eSUN |
Nozzle 240–260°C, bed 95–110°C, chamber 40–55°C, fan 0%.
Retraction 2 mm at 40 mm/s. Layer height 0.16–0.24 mm, infill 30%.
Yes: ASA requires an enclosure (40–55°C).